The coupler used to mount the 1/2 inch stainless steel shaft to the motor shaft. It uses 4 Allen set screws to hold it tightly onto the shafts. The two shafts are not the same diameters, so you may have to have this made at a local machine shop.

This picture has its own page with more detail, click here to see it.
This is a heavy-duty one-speed mixer, homemade, with a 1/3 hp motor. It can handle up to ten gallons of high-density glaze or body slurry.
| Articles |
A One-speed Lab or Studio Slurry Mixer
A single-speed lab mixer can be made for much less money than buying a commercial unit. Using it you can slurry up a 100 lb batch of porcelain powder in minutes and it will be smooth as silk. |