| Monthly Tech-Tip | No tracking! No ads! |
This is GR6-L Ravenscrag Raspberry glaze fired at cone 6 using the C6DHSC schedule. The body on the left is Plainsman M340. On the right is Coffee Clay. The black burning color of the Coffee Clay is due to a 10% raw umber addition, the manganese in the umber interacts on edges where it is thinner.
| Recipes |
GR6-L - Ravenscrag Cone 6 Transparent Burgundy
A stain-based method to achieve this color using the Ravenscrag base recipe. |
Buy me a coffee and we can talk