The clay body is Plainsman P700. This was fired in cone 10R using the C10RPL firing schedule. The outside glaze is G2571C. The inside glaze is G1947U.

This picture has its own page with more detail, click here to see it.
The clay is Plainsman H550 buff stoneware. The cone 10R firing schedule was C10RPL. The inside glaze is G1947U. 4% titanium and 0.5% cobalt oxide have been added to the base G2571A recipe. This G2571C thus inherits all the good properties of that parent base glaze.
| Materials |
Rutile
A raw TiO2-containing mineral used in ceramics to color and variegate glaze surfaces. |
| Materials |
Titanium Dioxide
A super white powder used in ceramic glazes to variegate, opacify and moderate color. |
| Glossary |
Rutile Blue Glazes
A type of ceramic glaze in which the surface variegates and crystallizes on cooling in the presence of titanium and iron (usually sourced by rutile) |