| Monthly Tech-Tip | No tracking! No ads! | 
This is P5867, a chocolate brown burning super-plastic base clay (to which 20% coarse grog is added) matures at cone 6. Yet this body is common used at cone 10R. The grog stabilizes the fired matrix enough that it stands up in the kiln. And it fires to a dense product that can withstand any weather. It does have a porosity of 4%, but that is coming from the grog. Several manufacturers around the world make bodies like this, some can have almost double the grog this one has. These two mugs employ engobes on the inside (a brown and a blue, applied at the leather hard stage - L3954N), enabling a smoother glaze surface.

This picture has its own page with more detail, click here to see it.
The super-smooth clay on the left is "Industrial Crank" from Potclays in the UK, I have removed the grog (our test code number L3868). First I did our standard tests on that body, then I dried some, slaked it in water, screened the grog out and then dewatered the remaining clay to plastic form. The grog yielded weighed the same as the clay portion of the recipe yet this body is known for amazing workability and toughness! How is that possible with so much aggregate in the recipe? The base clay body is extremely smooth, sticky and highly plastic. Mixtures of just ball clay and feldspar (e.g. 75:25) will yield this type of material, some ball clays will produce as little as 6% drying shrinkage using this ratio. The grog they use is also special: The particles have angular shapes and a narrow range of sizes, from about 35 mesh to 70 mesh (most is of the coarsest size). This narrow range of sizes means dramatically less particle surface area. These factors produce much less disruption of the plastic properties of the base clay. How could you make a body like this? Slurry up about 75% ball clay and 25% feldspar and wedge the grog into that.
| Articles | Outdoor Weather Resistant Ceramics How can you be sure that the porosity of your fired ceramic ware is low enough to prevent freeze-thaw breakdown in the winter? | 
| Glossary | Vitrification A process that happens in a kiln, the heat and atmosphere mature and develop the clay body until it reaches a density sufficient to impart the level of strength and durability required for the intended purpose. Most often this state is reached near zero p | 
Buy me a coffee and we can talk