Two cats made with the Tin Foil base and about 4% red copper oxide. Both of these show the lovely green you can get with copper. Both were fired in a gas kiln; the cat on the left was at the edge of a shelf, close to the flame. The cat on the right was in the center of the shelf. Both were cast of White Stallion porcelain.
| Recipes |
TNF2CG - Tin Foil II Crystalline Glaze
Cone 6-9 - Dolomite, tin, titanium variant |