To recover the material on the screen we wash it backwards into a container (turning the sieve to catch it all).
| Projects |
Testing a New Load of EP Kaolin
Kaolins can vary in many ways. Yet they are the foundation of all porcelain and light stoneware clay body recipes. It is vital to test each incoming shipment of material. Problematic brands can even require some testing on every pallet. |
| Glossary |
Particle Sizes
Knowledge of the physical and ultimate particles sizes in ceramic minerals and materials is an important part of understanding them, predicting their usefulness and explaining their behavior. |