| Monthly Tech-Tip | No tracking! No ads! |
I had this done at Shapeways.com. They offer an after-print polishing service, which I did not get. The plastic one on the left (actually printed from PLA filament) weighs 5 grams. The steel one weighs 45 grams! It cost $35 to print this. The quality is like regular stainless, this is incredibly hard! Fitting it on the shaft was the first issue. The shaft measures 8mm. My drawing sets the hole at 7.9mm (5/16"). On the 3D print with PLA I got 7.8mm, but this this arrived at 7.7mm. It required a lot of work to enlarge the hole to fit. Thus, if I were to print this again, I would set the drawing at 8.2. That should either fit or only require enlarging the hole slightly (using emery cloth). The second issue was the hole and tap for the set screw. Drilling it was very hard, the first bit broke. The second made it through, but we could not tap the threads. So we will glue it to the shaft. Do you have a suggestion on a better way to fix it to the shaft? Please let me know.
| Articles |
A One-speed Lab or Studio Slurry Mixer
A single-speed lab mixer can be made for much less money than buying a commercial unit. Using it you can slurry up a 100 lb batch of porcelain powder in minutes and it will be smooth as silk. |
| Glossary |
Propeller Mixer
In ceramic studios, labs and classrooms, a good propeller mixer is essential for mixing glaze and body slurries. |
Buy me a coffee and we can talk