| Monthly Tech-Tip | No tracking! No ads! |
This has surpassed the old Octal on my list of favorites and it's my base of choice for workshops. Many variations and revisions of this recipe are covered in book 1 and 2.
Bory 1 produces crystals in profusion, but only rarely does it cover a surface completely. If you prefer to see a lot of ground, this is a good choice.
| Recipes |
BORY1 - Bory 1 Crystalline Glaze
Cone 6-10 - Added Gerstley Borate lowers temperature to cone 6, titanium to seed crystals |
Buy me a coffee and we can talk