| Monthly Tech-Tip | No tracking! No ads! |
The blue second layer here is 5x20 cone 6 clear with 2% cobalt oxide and 5% rutile. The base black glaze is 5x20 with 4% Mason 6666 stain.
| Recipes |
G1214M - 20x6 Cone 6 Base Glossy Glaze
A recipe developed by Tony Hansen in the 1980s. Its was popular for the simplicity and how well it worked with chrome-tin stains. It was upgraded many times. |