| Monthly Tech-Tip | No tracking! No ads! |
These mugs are on a plaster table, freshly thrown on the wheel. I made the box cover from a large sheet of cardboard and painted wax emulsion on the inside. When left overnight under the box the mugs dewater evenly, the plaster pulls water from the air in the box and directly from the thicker bases. If I am worried they will stiffen too much overnight I water down the plaster to keep the humidity. When things are right, in the morning they are stiff enough for handle attachment and to turn over to ready them for trimming. An advantage of this method is that I can throw ware minutes before closing time, come back in the morning, and they are ready. And pieces do not experience the unevenness in drying that happens typically when pieces are left to air dry (after throwing) until they are stiff enough to support a cloth and plastic to cover them.
| Articles |
Drying Ceramics Without Cracks
Anything ceramic ware can be dried if it is done slowly and evenly enough. To dry faster optimize the body recipe, ware cross section, drying process and develop a good test to rate drying performance. |
| Glossary |
Plaster table
Essential in a pottery studio for dewatering reclaim clay, stiffening clay that is too soft or making your own clay bodies. |
Buy me a coffee and we can talk