| Monthly Tech-Tip | No tracking! No ads! |
The 20cm vase on the left is thrown from what I thought was a very plastic body, M370. I achieved close to the same thickness top-to-bottom (5mm). The one on the right was the same original height, 20cm. But it has dried down to only 18cm high, it shrinks 14% (vs. 6% for the other). The thinnest part of the wall is near the bottom, only 2mm thick! How is it possible to throw that thin? The body is 50% ball clay and 50% bentonite. Bentonite, by itself, cannot be mixed with water, but dry-blended with fine-particled ball clay it can. That bentonite is what produces this magic plasticity. But it comes at a cost. It took about four days to dewater the slurry on our plaster table. And one month under cloth and plastic to dry it without cracks.
| Articles |
Drying Ceramics Without Cracks
Anything ceramic ware can be dried if it is done slowly and evenly enough. To dry faster optimize the body recipe, ware cross section, drying process and develop a good test to rate drying performance. |
| Glossary |
Plasticity
Plasticity (in ceramics) is a property exhibited by soft clay. Force exerted effects a change in shape and the clay exhibits no tendency to return to the old shape. Elasticity is the opposite. |
| Materials |
Bentonite
Bentonite can make a clay body instantly plastic, only 2-3% can have a big effect. It also suspends slurries so they don't settle out and slows down drying. |
Buy me a coffee and we can talk