Look at how fluid G3879 is at cone 06 even though it has the Al2O3 and SiO2 of a cone 6 (or even cone 10 glaze)! It have found that glazes with lots of boron can tolerate amazingly high levels of Al2O3 and SiO2 and still melt very well. And they create many options to lower thermal expansion that would not otherwise be available. The G3806N recipe has the amazing ability to tolerate large additions of kaolin. Each addition sacrifices some melt fluidity but the glaze stays glossy and gets more durable (because of the increased Al2O3 and SiO2). And the thermal expansion drops even more. A highly melt fluid, super gloss with low thermal expansion is super difficult at cone 6, but here it is. The secret is high boron. From frits.
| Recipes |
G3879 - Cone 04 Transparent Low-Expansion transparent glaze
A super transparent low fire base clear glaze created by reverse engineering a commercial product. |
| Glossary |
Glaze Durability
Ceramic glazes vary widely in their resistance to wear and leaching by acids and bases. The principle factors that determine durability are the glaze chemistry and firing temperature. |
| Oxides | Al2O3 - Aluminum Oxide, Alumina |
| Oxides | SiO2 - Silicon Dioxide, Silica |
Buy me a coffee and we can talk