This can fire almost black on reduction. However, as a pure material, it is prone to dunting as it is high in larger quartz particles.

This picture has its own page with more detail, click here to see it.
This is a high iron two-material stoneware fired in reduction, purely a test body we are working on. Normally such bodies are rendered unsuitable because of black coring associated with FeO. But 10% added Custer Feldspar solves that problem, combining with the iron to vitrify the body to excellent fired strength (it does have 5% porosity but this is mainly due to the cavities formerly occupied by the iron pyrite particles. The color and iron speckle are contributed by both of the raw materials in the body. Saint Rose Red supplies most of the iron to produce the red coloration. A1 bentonitic clay adds plasticity and contributes the pyritic iron particles. The fired bars of this body show it at cone 10 reduction (top) and cone 10 oxidation down to 7 (downward from top). Adding just a little more feldspar produces a metallic firing surface! The glaze is GR10-CW, pure Ravenscrag Slip with 10% talc opacified with a little Zircopax and tin oxide.
| Materials |
Fire-Red
|
Buy me a coffee and we can talk