| Monthly Tech-Tip | No tracking! No ads! |
A comparison of the plasticity of two bentonites was done by diluting them with silica. The top sample is Volcay 325 mixed 25:75 with silica. It is a standard Wyoming sodium bentonite - mined, dried and ground. The bottom specimen is Hectalite 200, a highly refined white hectorite, mixed 50:50 with silica. Notice how much less plastic it is (even though at double the percentage).
| Materials |
Hectalite 200
|
| Materials |
Volclay Bentonite
|
| Materials |
Bentonite
Bentonite can make a clay body instantly plastic, only 2-3% can have a big effect. It also suspends slurries so they don't settle out and slows down drying. |
| Glossary |
Plasticity
Plasticity (in ceramics) is a property exhibited by soft clay. Force exerted effects a change in shape and the clay exhibits no tendency to return to the old shape. Elasticity is the opposite. |