Robin's egg blue at Cone 10R: add 1% cobalt oxide and 0.2% chrome oxide to GR10-J Ravenscrag silky matte. Does not work well on porcelains (left), very well on buff stonewares (right). Inside of center mug is GR10-J.
| Recipes |
GR10-J - Ravenscrag Cone 10R Dolomite Matte
Plainsman Cone 10R Ravenscrag Slip based glaze. It can be found among others at http://ravenscrag.com. |