| Monthly Tech-Tip | No tracking! No ads! |
These are fired bars of Laguna SG758 Barnard Slip substitute going from cone 04 (bottom) to cone 6 (top). It is melting at cone 6. The bars are expanded above cone 6 and becoming quite porous. The drying shrinkage is around 7%, it is quite plastic.
| Glossary |
Material Substitution
Material substitutions in ceramic glaze and body recipes must consider their chemistry, mineralogy and physical properties |
| Materials |
SG 758
|
Buy me a coffee and we can talk