There is nothing like feeling the texture of a clay body on a potter's wheel to judge the suitability of its particle size distribution. What you feel is sometimes different than PSD data may suggest. That texture can be recorded in your Insight-live account as a photo if you snap a closeup of the rim like this. I am testing the plastic character of a new mining of one of our clay materials and need to judge its texture in comparison with the existing one. In this case, these side-by-side photos confirm my other observations.
| Glossary |
Particle Sizes
Knowledge of the physical and ultimate particles sizes in ceramic minerals and materials is an important part of understanding them, predicting their usefulness and explaining their behavior. |