| Monthly Tech-Tip | No tracking! No ads! |
Notice how the bubbling from the off-gassing of the manganese has variegated the surface.
| Glossary |
Reactive Glazes
In ceramics, reactive glazes have variegated surfaces that are a product of more melt fluidity and the presence of opacifiers, crystallizers and phase changers. |
| Materials |
Manganese Dioxide
A source of MnO used in ceramic glazes and the production of ceramic stains. Commonly made by grinding pyrolusite rock. |