| Monthly Tech-Tip | No tracking! No ads! |
(50:50 Ravenscrag Slip:Alberta Slip) at cone 10R on porcelain (right) and stoneware (left).
| Recipes |
GR10-E - Alberta Slip:Ravenscrag Cone 10R Celadon
A celadon recipe affording slurry and fired properties control (because proportions of raw and calcined materials and frit can be adjusted) |
| Glossary |
Celadon Glaze
A type of stoneware glaze normally fired in a high temperature reduction atmosphere kiln. It is transparent and stained green or blue by the presence of iron oxide. |