Cone 5 GR6-A glaze at cone 5R on Plainsman M340 (left) and pure Ravenscrag Slip at cone 10R on H550 (right).
| Recipes |
GR6-A - Ravenscrag Cone 6 Clear Glossy Base
This Plainsman Cone 6 Ravenscrag Slip base is just the pure material with 20% added frit to make it melt to a glossy natural clear. |