| Monthly Tech-Tip | No tracking! No ads! |
This is G3806F copper green glaze. It is highly melt fluid at cone 6. As the glaze begins to melt notice that it splits on the sharp concave sections on the handle join. The underscore the needs for the melt to be sufficiently fluid to flow back in and heal these areas.
| Glossary |
Melting Temperature
The melting temperature of ceramic glazes is a product of many complex factors. The manner of melting can be a slow softening or a sudden liquifying. |
Buy me a coffee and we can talk