| Monthly Tech-Tip | No tracking! No ads! |
The cone 6 G1214M glaze on the left melts well. Can it benefit from a silica addition? Yes. The right adds 20% yet still melts as well, covers better, is more glossy, more resistant to leaching, harder and has a lower thermal expansion.
| Oxides | SiO2 - Silicon Dioxide, Silica |
| Oxides | Al2O3 - Aluminum Oxide, Alumina |
| Recipes |
G1214M - 20x6 Cone 6 Base Glossy Glaze
A recipe developed by Tony Hansen in the 1980s. Its was popular for the simplicity and how well it worked with chrome-tin stains. It was upgraded many times. |
| Glossary |
Silica:Alumina Ratio
A formula ratio used to evaluate and predict firing properties in ceramic glazes. |
| Glossary |
Food Safe
Be skeptical of claims of food safety from potters who cannot explain or demonstrate why. Investigate the basis of manufacturer claims and labelling and the actual use to which their products are put. |
| Articles |
G1214M Cone 5-7 20x5 glossy transparent glaze
This is a base transparent glaze recipe developed for cone 6. It is known as the 20x5 or 20 by 5 recipe. It is a simple 5 material at 20% each mix and it makes a good home base from which to rationalize adjustments. |
Buy me a coffee and we can talk