| Monthly Tech-Tip | No tracking! No ads! |
A 13 inch vase glazed with 100% Alberta Slip fired at cone 10R. The glaze was sprayed on. It is about 60% calcine and 40% raw powder. When it is very thin, as on the shoulder, it is quite metallic and varies from deep red to brown (depending on thickness). Where thick it is a tenmoku high gloss. The spots on the shoulder are thicker areas that have glossed.
| Recipes |
GA10-A - Alberta Slip Base Cone 10R
Alberta Slip at 60:40 calcine:raw makes a great tenmoku-like glaze at cone 10R |