| Monthly Tech-Tip | No tracking! No ads! |
It is old, but nothing we have ever used fires as evenly and reliably as this downdraft kiln. It was built by Luke Lindoe in the 1960s. I have used it through my entire life as a potter since the early 1970s. Two burners at 2 inches oil-column will take it to 1000F fairly quickly, but it takes 4 burners at 4 inches and 20 hours to get it to cone 10. I can judge the back pressure and degree of reduction by the length and color of the flames at the peepholes and color of the flame passing the damper at the back. Changing the damper position by an eighth of an inch during reduction is enough to discern a change in the flame.
| Firing Schedules |
Plainsman Cone 10R Firing
Six-step oxidize-at-end schedule to 2372F |
| Articles |
Building a Lindoe Downdraft Gas Kiln
|
Buy me a coffee and we can talk