This is 85% Alberta Slip, 11% lithium and 4% tin fired at cone 6 in oxidation. Like the original Albany version, it has a very low thermal expansion (because of the high lithium content) and likes to shiver on many clay bodies.

This picture has its own page with more detail, click here to see it.
These mugs have experienced very serious shivering. This is an Albany Slip glaze with 10% lithium carbonate, it is known to have a very low thermal expansion. This problem can be solved by reducing the amount of lithium or adding high-expansion sodium or potassium. However these fixes will likely affect the appearance.
| Media |
Replace Lithium Carbonate With Lithium Frit Using Insight-Live
Raw lithium carbonate can often be replaced with a lithium-containing frit if you can do the chemistry. And you can at insight-live.com. |
| Articles |
Alberta Slip, 20 Years of Substitution for Albany Slip
Alberta Slip makes a great base for glazes because not only is it almost a complete glaze by itself but it has low thermal expansion, it works well with frits and slurry properties can be adjusted. |
| Recipes |
GA6-G - Alberta Slip Lithium Brown Cone 6
Plainsman Cone 6 Alberta Slip based glaze. |
| Materials |
Lithium Carbonate
A powerful melter very valuable in ceramic glazes. It is 40% Li2O and has an LOI of 60% (lost as CO2 on firing). This material in now incredibly expensive. |
| Materials |
Alberta Slip
Albany Slip successor - a plastic clay that melts to dark brown glossy at cone 10R, with a frit addition it can also host a wide range of glazes at cone 6. |