| Monthly Tech-Tip | No tracking! No ads! |
This is a cone 6 stoneware with 0.3% 60/80 mesh manganese granular (Plainsman M340). Fired from cone 4 (bottom) to cone 8 (top). This body is normally stable to cone 8, but with the manganese it begins to bloat at cone 7! This is evidence that particles of manganese are generating gases as they decompose and melt at the same time as the body is vitrifying, these produce volumes and pressures sufficiently suddenly that closing channels within the maturing body are unable to vent them out.
| Materials |
Manganese Granular
In ceramics, it is used primarily in clays and glazes to achieve fired speckle (including the brick industry). |
| Hazards |
Manganese in Clay Bodies
Manganese is used to stain clays (using black) and to impart fired speckling (as a decorative effect). It is dangerous? |
| Temperatures | Manganese compounds may begin to fume (932-) |
| Troubles |
Bloating
Bloating occurs when the off-gassing of decomposing particles in a body has not completed by the onset of density and impermeability associated with the vitrification process. |
| Glossary |
LOI
Loss on Ignition is a number that appears on the data sheets of ceramic materials. It refers to the amount of weight the material loses as it decomposes to release water vapor and various gases during firing. |