Since iron oxide is a strong flux in reduction, iron-based pigments can run badly if applied too thickly.
| Materials |
Iron Oxide Red
Red iron oxide is the most common colorant used in ceramic bodies and glazes. As a powder, it is available in red, yellow, black and other colors. |