| Monthly Tech-Tip | No tracking! No ads! |
Plainsman M390 with 12.5% 48 mesh kyanite wedged in. This was added to improve the drying properties while maintaining the plasticity. However, the throwing also improved! It was easier to pull up into a tall cylinder. The surface texture is only moderately disrupted by a slight graininess.

This picture has its own page with more detail, click here to see it.
This is the surface after trimming. M390 is normally smooth. It is plastic enough to be able to tolerate this grog without apparent loss in workability (still throwing well). And it does not feel overly abrasive on the wheel (unless your hand goes down onto the wheelhead). How is that possible? Although the particles of grog are large, they are not touching each other and readily press down into the clay.
| Materials |
Kyanite
Kyanite is a granular material used in the manufacture of ceramics and abrasives. It is notable for low thermal expansion and one-way expansion on heating. |
| Glossary |
Wedging
The process of mixing a plastic clay by hand before forming it. Similar to kneading of bread dough, it is considered an essential step by most potters. |