| Monthly Tech-Tip | No tracking! No ads! |
These mugs are the same clay and glazed with a 50:50 raw:calcine Alberta Slip mix (GA10-A) and fired to cone 10R. Both looked like the one on the left. The one on the right has a decal on the inside, it was fired to 1500F. This firing has made the glaze significantly glossier, darker, deeper and more vibrant. Why? I have no idea. I have 20 more using this glaze and made from this and other clays, they all did the same thing.
| Recipes |
GA10-A - Alberta Slip Base Cone 10R
Alberta Slip at 60:40 calcine:raw makes a great tenmoku-like glaze at cone 10R |
Buy me a coffee and we can talk