Made in 1982. Clay is Plainsman H443 fired at cone 10R. Glaze is G2571A with 0.25% chrome oxide, 1.0% cobalt oxide and 0.25% manganese granular. The decoration was done using a wax resist and throwing techniques learned from John Porter. During the early years, the big gas reduction kiln in the Plainsman studio was fired every month or two and each firing would have contained half a dozen of these, thus hundreds were made.
| Recipes |
G2571A - Cone 10 Silky Dolomite Matte glaze
A cone 10R dolomite matte having a pleasant silky surface, it does not cutlery mark, stain or craze on common bodies |