| Monthly Tech-Tip | No tracking! No ads! |
Fired at 1850F. Frit F-524 has run off the tester since 1850F. Frit 3602 is lead bisilicate.

This picture has its own page with more detail, click here to see it.
This cone 04 flow tester compares two commercial low-fire transparent glazes. Their different approaches to the chemistry are revealed by these melt flows. While 3825B appears to have a higher melt fluidity, its higher surface tension is the real story. This is demonstrated by how the flow meets the runway at a perpendicular angle. Notice that A, by contrast, meanders down the runway in a broad, flat and relatively bubble-free river. Low-fire glazes must pass many more bubbles than their high-temperature counterparts, the low surface tension of A aids in that. A is Amaco LG-10. B is Crysanthos SG213 (Spectrum 700 behaves similarly, although flowing less). Both have advantages and disadvantages and are worth testing in your application.
| Materials |
Ferro Frit 3602
|
| Materials |
Fusion Frit F-524
A low fire base glaze, add 10% kaolin, adjust thermal expansion using other frits. |
| Glossary |
Surface Tension
In ceramics, surface tension is discussed in two contexts: The glaze melt and the glaze suspension. In both, the quality of the glaze surface is impacted. |
Buy me a coffee and we can talk