| Monthly Tech-Tip | No tracking! No ads! |
I made the bottom and top radiuses and the height parametric. I made the diameter of the pouring ring = top diameter of the pot + 2 mm. The walls are 2mm thick because my 3D printer prints 0.4mm wide (that means two passes for each layer).
| Glossary |
0.8mm thickness
This is an ideal wall thickness to print on consumer 3D printer since to normally creates sufficient strength and prints in one two passes |
| Projects |
Nursery plant pot mold via 3D printing
|
Buy me a coffee and we can talk