| Monthly Tech-Tip | No tracking! No ads! |
Here GR6-M it is fired to cone 8 where the melt obviously has much more melt fluidity! The photo does not do justice to the variegation and crystallization happening on this surface. Of course, it is running alot more, so caution will be needed.
| Recipes |
GR6-M - Ravenscrag Cone 6 Floating Blue
Plainsman Cone 6 Ravenscrag Slip based version of the popular floating blue recipe. |
| Typecodes |
Floating Blue
A popular cone 6 glaze that employed Gerstley Borate, it was very troublesome to use and to fire. Much work has been done to create alternative recipes. |
| Glossary |
Reactive Glazes
In ceramics, reactive glazes have variegated surfaces that are a product of more melt fluidity and the presence of opacifiers, crystallizers and phase changers. |