| Monthly Tech-Tip | No tracking! No ads! |
The firing schedule for cone 5 was C5DHSC. The inside glaze is G2926B, outside is G2926B plus 10% Mason 6304 purple stain. There is no visible difference in the fired result.
| Glossary |
Cone 5
Also called "middle temperature" by potters, cone 5 (~2160F/1180C) refers to the low end of the temperature range at which most hobby and pottery stonewares and porcelains are fired. |
Buy me a coffee and we can talk