| Monthly Tech-Tip | No tracking! No ads! |
Three Cornwall Stone shipments (from 2011 and 2014) fired at cone 8 in melt flow GLFL testers and compared to Nepheline Syenite. Each contains 10% Ferro Frit 3134.
| Materials |
Cornwall Stone
|
| Materials |
Nepheline Syenite
|
| Materials |
Covia Nepheline Syenite
|
| Glossary |
Melt Fluidity
Ceramic glazes melt and flow according to their chemistry, particle size and mineralogy. Observing and measuring the nature and amount of flow is important in understanding them. |