| Monthly Tech-Tip | No tracking! No ads! |
This is G2571A cone 10R dolomite matte on an ironware body made from native North Carolina clays. Few glazes have the pleasant silky feel that this has yet are still functional. The feldspar content in the body has been tuned to establish a compromise between the warmer color that low percentages have with the higher strength that higher percentages enable. Careful porosity tests were done and recorded in an account at insight-live.com. The objective was to bring the body close to 3% absorption.
| Glossary |
Dolomite Matte
Dolomite matte glazes have the potential to be very silky and pleasant to the touch, while at the same time being hard, durable and non-crazed (if they are formulated correctly). |
| Glossary |
Functional
A term used in ceramic to express the degree to which an item is safe and stands up to everyday use. Functionality embodies strength, hardness, resistance to acid attack and thermal shock, etc. |