Strontium carbonate fired at 1800F and then allowed to rehydrate in the air for two days. It is crumbling like this all by itself, similar to what calcium carbonate does as it rehdrates.
| Materials |
Strontium Carbonate
A pure source of SrO for ceramic glazes. It contains 70% SrO and has an LOI of 30% (released as CO2 during firing). |