| Monthly Tech-Tip | No tracking! No ads! |
Fired at cone 10R. The GR10-C Raven-Talc matte is just 90% Ravenscrag Slip and 10% talc. This produces a stunning silky, variegated surface (which could be a base for many colorants). The GR10-J Raven-Dolomite matte was patterned after our G2571A glaze, but using as much Ravenscrag Slip in the recipe as possible while maintaining the same chemistry (its surface is less variegated and more matte).
| Recipes |
GR10-C - Ravenscrag Cone 10R Silky Talc Matte
Just Ravenscrag Slip plus 10% talc produces a visually variegated surface that feels silky and looks stunning! |