| Monthly Tech-Tip | No tracking! No ads! |
This was left for 24 hours. Wrapped in stretch wrap. Then the surface of the glaze was inspected under a lamp to detect any differences between the lemoned and non-lemoned surfaces. Lemons are highly acidic. This glaze passed because the base recipe, G3806N, was methodically developed so that it has plenty of Al2O3 and SiO2 (in the fired chemistry) to build a stable glass.
| URLs |
https://insight-live.com/insight/share.php?z=gbcM8HXmX2
2019 Development of G3806 melt-fluid low-expansion clear base glaze |
| Hazards |
Copper Oxide and Carbonate
|
| Tests |
Glaze Leaching Test
Simple tests to evaluate the stability of a ceramic or pottery glaze against leaching metals in food or drink. |