Alberta slip melts well with very little frit at cone 6
| Articles |
Alberta Slip, 20 Years of Substitution for Albany Slip
Alberta Slip makes a great base for glazes because not only is it almost a complete glaze by itself but it has low thermal expansion, it works well with frits and slurry properties can be adjusted. |
| Articles |
Duplicating Albany Slip
How Alberta Slip was created by analysing and duplicating the physical and chemical properties of Albany Slip |