I am going to fire them at about 10 temperatures starting at cone 022. These will be a great to determine whether they suddenly melt or slowly soften over a range of temperatures. I will be able to see how wide that range is and how they behave as they go beyond it. I also included Gerstley Borate, mother nature's nature boron source. They way it melts should clear contrast with the frits.
| Projects |
Comparing the Melt Fluidity of 16 Frits
|