| Monthly Tech-Tip | No tracking! No ads! |
Cone 10R top, 11 oxidation and downward below that. This material, although called a "fireclay", is more fine grained and much more vitreous than what would normally be considered a refractory fireclay. Is it similar to Lincoln Fireclay (from California).
| Materials |
Imco 400 Fireclay
|
| Glossary |
Refractory
In the ceramic industry, refractory materials are those that can withstand a high temperature without deforming or melting. Refractories are used to build and furnish kilns. |
| Glossary |
Fireclay
A clay that withstands fire. In the ceramics industry, clays that are resistant to deforming and melting at high temperatures are called fireclays. Kiln bricks are often made from fireclay. |
Buy me a coffee and we can talk