| Monthly Tech-Tip | No tracking! No ads! |
A transparent glazed. It is a made from Plainsman Polar Ice in 2014 (a New Zealand kaolin based translucent porcelain) and fired to cone 6 with G2926B clear glaze. 5% Mason 6306 teal blue stain was added to the clay, then this was wedged only a few times. The piece was thrown, then trimmed on the outside at the leather hard stage and sanded on the inside when dry.
| Glossary |
Marbling
In ceramics, bodies of different colours can be kneaded together to produce a marble-like result. But caution is needed. |
| Materials |
New Zealand Halloysite
The whitest burning kaolin we have ever seen. It is very sticky when wet, suspends glazes well & makes super white porcelain (with help from a white bentonite). |