The clear glaze is G1916Q. Fired at cone 04. The body on the left is 50:50 Old Hickory M-23 ball clay and Cimtuff talc. The body on the right is a mix of KT1-4 ball clay and C-98 talc. It is firing whiter. But this is not only because of the talc, the KT1-4 ball clay is whiter-burning than the M23.
| Materials |
Cimtuff 9115 Talc
|
| Materials |
Natural Talc C-98
|