| Monthly Tech-Tip | No tracking! No ads! |
Round or square fired bars are subject to a force that tests their tensile strength. The strength can be calculated from the force and the dimensions of the cross section where the break occurred.
| Tests |
Fired Strength Round Bars
|
| Tests |
Dry Strenth (Round Bars)
|
| Tests |
Dry Strength (kgf/cm2)
Measure the tensile strength of a dried clay test bar |
| Tests |
Dry Strength (Square Bars)
Measure the tensile strength of a square cross section test bar |
| Tests |
Fired Strength Square Bars
|
| Glossary |
Fired Strength
Ceramics, by their brittle nature, have high compressive strength. But in functional ceramics we are more concerned about the tensile strength as this relates better to serviceability. |