The Veegum is dense and white, but not melting. The Mineral Colloid fires like a typical raw bentonite (dark brown, high soluble salts and beginning to melt). The Gelwhite is completely melted and foamed.
| Materials |
Mineral Colloid BP
|
| Materials |
Gelwhite H
|
| Materials |
Bentone MA
|
| Materials |
Veegum
A clay of incredibly small particle size. It has the highest plasticity of any known clay and acts as a suspending and gelling agent in slurries. |