These mugs are intended to demonstrate the techniques, recipes and materials I promote on this site. My audience is potters, hobbyists and manufacturers. Each mug described maintains its own permanent page here with detailed physical description as well as information on every detail of how it was made. Since each has links into many areas of this site that provide more detail, researching just one mug could take hours! The "AJxxxx" serial number on any can be searched here.
Serial Number: AJ24316
Run/Test Number: P6932
Technique: Thrown, incised, liner-glazed inside, dip-glazed outside
Firing Schedule - C6DHSC
Temperature - Cone 6
Glaze Inside - G2926B
Glaze Outside - G2926B Purple
Clay Body - M370
Foot Style - Fluted ring
Width at rim (perpendicular to handle) - 101 mm (4.0 in)
Depth at rim (including handle) - 130 mm (5.1 in)
Height - 118 mm (4.6 in)
Weight - 356 grams (12.5 oz)