2380 | 2378 | 2382 | 2385 | 2383 | 2386 | 2381 | 2379 | 2388 | 2466 | 2461 | 2470 | 2469 | 2452 | 2463 | 2455 | 2454 | 2460 | 2458 | 2465 | 2467 | 2457 | 2436 | 2437 | 2444 | 2447 | 2441 | 2448 | 2428 | 2340 | 2342 | 2358 | 2393 | 2397 | 2398 | 2400 | 2402 | 2403 | 2406 | 2416 | 2414 | 2409 | 2415 | 2411 | 2433 | 2422 | 2429 | 2431 | 2432 | 2361 | 2476 | 2477 | 2478 | 2489 | 2487 | 2490 | 2493 | 2488 | 2491 | 2479 | 2480 | 2474 | 2475 | 2350 | 2362 | 2367 | 2369 | 2355 | 2366 | 2345 | 2346 | 2352 | 2353 | 2394 | 2392 | 2391 | 2360 | 2343 | 2430 | 2453 | 2456 | 2462 | 2442 | 2446 | 2472 | 2471 | 2389 | 2505 | 2499 | 2510 | 2507 | 2511 | 2514 | 2504 | 2417 | 2376 | 2374 | 2375 | 2275 | 2549 | 2541 | 2537 | 2551 | 2538 | 2540 | 2539 | 2542 | 2543 | 2547 | 2546 | 2550 | 2545 | 2544 | 2533 | 2518 | 2531 | 2525 | 2527 | 2522 | 2529 | 2535 | 2556 | 2559 | 2562 | 2563 | 2565 | 2567 | 2568 | 2570 | 2571 | 2572 | 2574 | 2573 | 2558 | 2586 | 2585 | 2584 | 2583 | 2582 | 2588 | 2577 | 2576 | 2575 | 2591 | 2592 | 2587 | 2548 | 2368 | 2371 | 2532 | 2372 | 2520 | 2523 | 2405 | 2401 | 2459 | 2344 | 2341 | 2553 | 2561 | 2581 | 2580 | 2579 | 2578 | 2384 | 2348 | 2351 | 2390 | 2359 | 2339 | 2347 | 2404 | 2425 | 2424 | 2426 | 2427 | 2420 | 2419 | 2418 | 2281 | 2423 | 2421 | 2438 | 2443 | 2445 | 2440 | 2451 | 2481 | 2482 | 2484 | 2483 | 2485 | 2495 | 2508 | 2509 | 2552 | 2370 | 2373 | 2516 | 2554 | 2502 | 2494 | 2410 | 2407 | 2408 | 2569 | 2557 | 2519 | 2357 | 2503 | 2530 | 2349 | 2289 | 2536 | 2560 | 2555 | 2521 | 2589 | 2515 | 2601 | 2603 | 2604 | 2605 | 2606 | 2607 | 2608 | 2609 | 2610 | 2611 | 2613 | 2513 | 2614 | 2616 | 2617 | 2618 | 2619 | 2620 | 2621 | 2622 | 2623 | 2624 | 2625 | 2626 | 2627 | 2628 | 2629 | 2630 | 2631 | 2632 | 2633 | 2634 | 2602 | 2635 | 2636 | 2637 | 2639 | 2640 | 2642 | 2643 | 2399 | 2387 | 2354 | 2377 | 2449

These mugs are intended to demonstrate the techniques, recipes and materials I promote on this site. My audience is potters, hobbyists and manufacturers. Each mug described maintains its own permanent page here with detailed physical description as well as information on every detail of how it was made. Since each has links into many areas of this site that provide more detail, researching just one mug could take hours! The "AJxxxx" serial number on any can be searched here.

White glazed speckled stoneware mug

Serial Number: AJ24439
Run/Test Number: L4471J2
Technique: Thrown, incised, dip-glazed

Firing Schedule - PLC6DS
Temperature - Cone 6
Glaze Inside - G3926B
Glaze Outside - G3926B
Clay Body - M340S
Foot Style - Fluted ring
Width at rim (perpendicular to handle) - 95 mm (3.7 in)
Depth at rim (including handle) - 131 mm (5.2 in)
Height - 122 mm (4.8 in)
Weight - 369 grams (13.0 oz)

Price: $40.00 - Buy it