These mugs are intended to demonstrate the techniques, recipes and materials I promote on this site. My audience is potters, hobbyists and manufacturers. Each mug described maintains its own permanent page here with detailed physical description as well as information on every detail of how it was made. Since each has links into many areas of this site that provide more detail, researching just one mug could take hours! The "AJxxxx" serial number on any can be searched here.
Serial Number: AJ24345
Run/Test Number: L4239
Technique: Jiggered, dip-glazed, cast handle
Firing Schedule - C10RPL
Temperature - Cone 10R
Glaze Inside - G2571A Bamboo
Glaze Outside - G2571A bamboo matte
Clay Body - H550 Casting
Foot Style - Fluted ring
Width at rim (perpendicular to handle) - 94 mm (3.7 in)
Depth at rim (including handle) - 122 mm (4.8 in)
Height - 110 mm (4.3 in)
Weight - 428 grams (15.1 oz)
Price: $35.00 - Buy it