These mugs are intended to demonstrate the techniques, recipes and materials I promote on this site. My audience is potters, hobbyists and manufacturers. Each mug described maintains its own permanent page here with detailed physical description as well as information on every detail of how it was made. Since each has links into many areas of this site that provide more detail, researching just one mug could take hours! The "AJxxxx" serial number on any can be searched here.
Serial Number: AJ24022
Run/Test Number: L3924C
Technique: Thrown, leather-hard under-glaze decorated, incised, 1650F bisque fired, dip-glazed
Firing Schedule - C04PLTP
Temperature - Cone 03
Glaze Inside - G2931K
Glaze Outside - G2931K
Clay Body - L3924C
Foot Style - Fluted ring
Width at rim (perpendicular to handle) - 83 mm (3.3 in)
Depth at rim (including handle) - 113 mm (4.4 in)
Height - 119 mm (4.7 in)
Weight - 312 grams (11.0 oz)